SA387Gr91CL2属于什么材质

产品信息

产品详细

SA387Gr9CL2与SA387Gr91CL2是铬钼耐热钢材质,适用于在高温下工作的焊接锅炉和压力容器,执行标准ASME SA387,ASTM A387/A387M-06a。

SA387Gr9CL2钢板应进行热处理:退火、或正火 回火,或当需方允许时,SA387Gr11Cl2可通过吹入空气或淬火(从奥氏体温度)来加速冷却,

随后进行回火,其回火温度应为:675℃

SA387Gr91CL2钢板应在1040-1080℃的范围内正火,并应在730-800℃的范围内回火

SA387Gr9CL2与SA387Gr91CL2化学成分比较(质量分数)/%

SA387Gr9CL2熔炼分析要求:

SA387Gr9CL2碳C:不大于0.15

SA387Gr9CL2硅Si:不大于1.0

SA387Gr9CL2锰Mn:0.3-0.6

SA387Gr9CL2磷P:不大于0.03

SA387Gr9CL2硫S:不大于0.03

SA387Gr9CL2铬Cr:8.0-10.0

SA387Gr9CL2钼Mo:0.9-1.1

SA387Gr9CL2钒V:不大于0.04

SA387Gr91CL2熔炼分析要求:

SA387Gr91CL2碳C:0.08-0.12

SA387Gr91CL2硅Si:0.2-0.5

SA387Gr91CL2锰Mn:0.3-0.6

SA387Gr91CL2磷P:不大于0.02

SA387Gr91CL2硫S:不大于0.01

SA387Gr91CL2铬Cr:8.0-9.5

SA387Gr91CL2钼Mo:0.85-1.05

SA387Gr91CL2钒V:0.18-0.25

SA387Gr91CL2镍Ni:不大于0.4

SA387Gr9CL2与SA387Gr91CL2钢板拉伸性能的比较

SA387Gr9CL2拉伸性能要求:

SA387Gr9CL2抗拉强度:515-690

SA387Gr9CL2屈服强度:不小于310

SA387Gr9CL2伸长率:不小于18

SA387Gr91Cl2拉伸性能要求:

SA387Gr91Cl2抗拉强度:585-760

SA387Gr91Cl2屈服强度:不小于415

SA387Gr91Cl2伸长率:不小于18

SA387Gr9CL2与SA387Gr91CL2的区号通过以上交货状态、熔炼分析、拉伸性能作比较可以看出,交货状态都是正火加回火,但两者的热处理工艺不同。熔炼分析可以看出SA387Gr91CL2对化学元素要求更严格,化学成分稍微不同。拉伸性能时完全不同,SA387Gr91CL2的屈服强度和抗拉强度要比SA387Gr9CL2要高。

 

 